Type: | C (Cast Iron Welding Rod) |
---|---|
Material: | Cast Iron |
Diameter: | 2.0-5mm |
Samples: |
---|
Customization: |
---|
Shipping Cost:
Estimated freight per unit. |
about shipping cost and estimated delivery time. |
---|
Payment Method: | |
---|---|
Initial Payment Full Payment |
Currency: | US$ |
---|
Return&refunds: | You can apply for a refund up to 30 days after receipt of the products. |
---|
Suppliers with verified business licenses
Hunan Xunzhuo Import & Export Co., Ltd.
Engine bases, gearcases and lathe guide rails.
stable arc, little spatter, less smoke;
higher deposition efficiency;
excellent welding performance;
easy restrike.
Z408 Cast Iron Welding Electrode
Accord with:GB/T 10044 EZNiFe-1
Equivalent norm: AWS A5.15 ENiFe-C1
Description:
Z408 is a graphitic (with strong reducing) type coating with Ni/Fe core welding electrodes for cast iron. It has features as follows: high toughness, excellent plasticity, low linear expansion coefficient, etc. Both AC and DC can be applied with welding.
Applications:
It is used for repairing welding important and high-toughness parts made of cast iron and modular iron, such as cylinder head, motor stand, gear wheel, etc.
Chemical Composition of Deposited Metal: (%)
|
C |
Mn |
Si |
S |
Ni |
Fe |
Al |
Cu |
Standard |
≤2.0 |
≤2.5 |
≤4.0 |
≤0.03 |
45-60 |
The rest |
≤1.0 |
≤2.50 |
Typical |
0.70 |
0.24 |
1.00 |
0.006 |
54 |
0.06 |
0.054 |
0.054 |
Recommended Current (AC or DC)
Size(mm) |
2.5*300 |
3.2*350 |
4.0*400 |
5.0*400 |
Current(A) |
50-80 |
80-110 |
110-140 |
150-180 |
Attention:
a. welding electrodes must be baked for 1 hour at the temperature of 150ºC before welding.
b. Small current is the best to be adopted.
Suppliers with verified business licenses